Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 171 MPa | 24800 psi | ASTM D638 |
Omni Plastics OmniLon™ 6 PA6 GR33 NA Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 171 MPa | 24800 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXS PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL36SXS is a compound based on PA 66 resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
Tensile Strength, Yield | 171 MPa | 24800 psi | ISO 527 |
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |