Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.00 MPa | 2466 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 115-1328 LMDPE Rotational Molding Resin Description: ICORENE 115-1328 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Tensile Strength, Yield | 17.00 MPa | 2466 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 115-1649 LMDPE Rotational Molding Resin Description: ICORENE 115-1649 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Tensile Strength, Yield | 17.00 MPa | 2466 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 115-1652 LMDPE Rotational Molding Resin Description: ICORENE 115-1652 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |