Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.9 MPa @Thickness 3.17 mm |
2450 psi @Thickness 0.125 in |
2"/min speed; ASTM D638 |
PolyOne Maxxam® DP 7916-2001 HIPS
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 16.9 MPa @Thickness 3.17 mm |
2450 psi @Thickness 0.125 in |
2"/min speed; ASTM D638 |
PolyOne Maxxam® RP81065 HIPS
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D638 |
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D638 |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D412 |
Teknor Apex APEX® 90-P513A-65-NT Polyvinyl Chloride+PUR Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | |
TriStar TriSteel PR Metal Backed PTFE Bearing System Ultraflon 602e enhanced PTFE (PR) lined metal backed bearing , high speed reciprocating, self lubricating, high temperature and high load applications. Liner is designed specifically for high freque.. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | |
TriStar TriSteel PT Metal Backed PTFE Bearing System Ultraflon 602 (PT) PTFE lined metal backed bearing system, low friction, high PV, high speed sleeve, flange and thrust bearings, zero lube required, high operating temperature. Ultraflon 602 PTFE Li.. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 8852 Moldings & Extrusions Flexible PVC General purpose compound recommended for extrusion applications. Contains a biocide and is UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 9149A Wire & Cable Flexible PVC Highly flame retardant tray cable (FT-4) jacket for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 18730 Wire & Cable Flexible PVC UL recognized 720 hour sunlight resistant in all colors, oil resistant, 105 C rated PVC jacket compound with good low temperature performance. Information provided by Georgia GulfGeorgia Gulf became.. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 19900 Wire & Cable Flexible PVC 105°C; VW-1 rated non-lead stabilized insulation with good flexibility. Ideally suited for 1/64 wall (18 AWG and larger). UL approved for TW, THW, THHW applications.Information provided by Georgi.. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 8880 Moldings & Extrusions Flexible PVC General purpose non-lead stabilized extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 19854 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound. Recognized by UL for TW and THW applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 2161A Wire & Cable Flexible PVC Flame retardant, oil resistant, 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D-638 |
Axiall 34431 Wire & Cable Flexible PVC TW insulation. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D638 |
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo.. |
|||
Tensile Strength, Yield | 16.9 MPa | 2450 psi | ASTM D638 |
Resirene Resirene® 2210 High Impact Polystyrene Features:Very High FlowEasy ProcessingGood GlossFlexibilityFDA Rating: 21 CFR 177.1640High ProductivityApplications:InjectionThin Wall ApplicationsHard to Fill MoldsTelephonical DevicesYot CupsToysC.. |