Polymer Property : Tensile Strength, Yield = 2420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.7 - 17.2 MPa
2420 - 2490 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 16.7 MPa
2420 psi
ASTM D412
Precision Polymer Engineering V60D Fluoroelastomer Compound
Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet Aerospace Specifications DTD5612A and DTD5543B Grade 60.Applications: Mouldings which are re..
Tensile Strength, Yield 16.7 - 17.2 MPa
2420 - 2490 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 16.7 MPa

@Thickness 3.20 mm
2420 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform..
Tensile Strength, Yield 16.7 MPa

@Thickness 3.20 mm
2420 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOL MC4352 PP+Rubber+MF
Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9..
Tensile Strength, Yield 16.7 MPa
2420 psi
ASTM D412
Teknor Apex Flexalloy® 3500-75 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
Tensile Strength, Yield 16.7 MPa
2420 psi
ASTM D412
Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 16.7 MPa
2420 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SFE 4500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Tensile Strength, Yield 16.7 MPa
2420 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SFE 5000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Tensile Strength, Yield 16.7 MPa
2420 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SIM 4029 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Tensile Strength, Yield 16.7 MPa
2420 psi
20 in/min; ASTM D638
Teknor Apex Sinvicomp SMG 5000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Tensile Strength, Yield 16.7 MPa
2420 psi
Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Tensile Strength, Yield 16.7 MPa
2420 psi
Zylog Hipolyene® GM BP 11 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Tensile Strength, Yield 16.7 MPa
2420 psi
at 300% elongation; ASTM D412
Lubrizol Estane® R190A Thermoplastic Polyurethane
Type: Estane® R190A is a Shore 93A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi..
Tensile Strength, Yield 16.7 MPa
2420 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SIH 5569 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Good Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: A; B; YI4; YI5 Agency Ratings: IEC 60502; VDE 0207 Forms: Pellets Processing ..