Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 600 A 33 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 600 A 33 Black 28 V Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ ND633 GF Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527-2/1A/5 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527 |
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha.. |
|||
Tensile Strength, Yield | 165 MPa @Strain 0.200 %, Temperature 870 °C |
23900 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes 25 alloy, vacuum investment castings, solution treated Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66 LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2300F PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2310 PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF33 L RD041 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: YellowTPCI# 8221102Information provi.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527-2 |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527 |
Eurostar Star L PA66 30V D61 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a PTFE/Silicone Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527 |
Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | |
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ISO 527-2/1A/5 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Tensile Strength, Yield | 165 MPa | 23900 psi | ASTM D638 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |