Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.9 MPa | 2300 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® D 4701 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good I.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 0302 PP NH Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingCoextrusionExtrusionUses:TubingPipingFurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098A-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | Longitudinal |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.003" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-412-98 |
Saint-Gobain Vendflow® E-70-V-CE Taste Barrier Tubing Formulation Description: Non-plasticized inner bore yeilds no taste: Vendflow® E-70-V-CE is specifically formulated to transfer water and beverages without imparting any "plastic" taste sometimes found in PV.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | at 200%; ASTM D412 |
Lubrizol Estane® ALR PC60D Thermoplastic Polyurethane Type: Estane® ALR PC60D is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableInformation Provided by The Lubrizol Corporation |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall EX1264 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for water stop applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall H 5177B Plenum Flexible PVC Plenum-grade jacket with good low temperature properties for use over 100% FEP primaries. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D412 |
ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generat.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 13820 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications. Good low temperature performance. Also suitable for outdoor jacket applicatio.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 13821 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 190 Moldings & Extrusions Flexible PVC 60C plug molding component. UL recognized component for 94 V-0 in all colors. 1.13 mm minimum thickness. UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axia.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 2110 Wire & Cable Flexible PVC Tray cable jacket for 105°C applications. Also suitable for direct burial applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gu.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 37740 Wire & Cable Flexible PVC 90°C rated compound designed for use as an inner and outer jacket in Teck 90 cables.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 38552 Wire & Cable Flexible PVC General purpose insulating and jacketing compound for 105°C AWM and SPT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 8803 Moldings & Extrusions Flexible PVC Microbe resistant extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets. Good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Ax.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 19850 Moldings & Extrusions Flexible PVC Primary insulation compound recommended for 105C, 1/32 wall and larger applications. Also well suited for plug molding. UL rated 94 HB.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | 2"/min; ASTM D638 |
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | TM R050-36 |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 02520 Plenum Flexible PVC Non-lead stabilized plenum grade jacket with good low temperature properties. Recommended for Category 5 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2.. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D-638 |
Axiall 8863 Moldings & Extrusions Flexible PVC A vinyl elastomer extrusion compound with rubber-like properties. Ideally suited for extruded profiles and tubings. Meets the requirements for LP Gas hose per UL21.Information provided by Georgia .. |
|||
Tensile Strength, Yield | 15.9 MPa | 2300 psi | ASTM D638 |
Multibase Multi-Flam™ 0107 HDPE Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingCoextrusionExtrusionUses:TubingPipingInformation provided by Multibase |