Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1517 - 1689 MPa | 220000 - 245000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | 1517 MPa | 220000 psi | Longitudinal |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Tensile Strength, Yield | 1517 MPa | 220000 psi | Transverse |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 13.5 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Tensile Strength, Yield | 1517 MPa | 220000 psi | |
HP Alloys Alloy 718, 25% Cold Worked, Aged 25% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Tensile Strength, Yield | 1517 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Yield | 1520 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
when tempered at 400°F |
Carpenter S7 Alloy Tool Steel (AISI S7) Carpenter S7 is a general purpose air hardening tool steel having high impact and shock resistance. It has good resistance to softening at moderately high temperatures. This combination of propertie.. |
|||
Tensile Strength, Yield | 1520 MPa | 220000 psi | R<sub>p</sub>02. 52 HRC. |
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Tensile Strength, Yield | 1517 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 4340 Specialty Steel, Heat Treatment: 899°C (1650°F) Q+T Data provided by Allvac.Applications: Rocket motor cases, ordnance hardware, aircraft structural components, transmission gears, components, fasteners. |
|||
Tensile Strength, Yield | 1517 MPa @Strain 0.200 % |
220000 psi @Strain 0.200 % |
|
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Tensile Strength, Yield | 1520 MPa | 220000 psi | R<sub>p</sub>02. 52 HRC. |
Assab Steels 8407 SUPREME Hot Work Steel 8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and .. |
|||
Tensile Strength, Yield | 1517 MPa | 220000 psi | Transverse |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Tensile Strength, Yield | 1517 MPa | 220000 psi | Longitudinal |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |