Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1335 MPa @Strain 0.200 % |
193600 psi @Strain 0.200 % |
|
Haynes 214® alloy, 50% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |