Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1320 MPa @Strain 0.200 %, Temperature 595 °C |
191000 psi @Strain 0.200 %, Temperature 1100 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |