Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.30 MPa
189 psi
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material..