Tensile Strength, Yield 1270 MPa

@Strain 0.200 %
184000 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 25% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 1270 MPa
184000 psi
R<sub>p</sub>02. 45 HRC.
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Tensile Strength, Yield 1270 MPa

@Strain 0.200 %
184000 psi

@Strain 0.200 %
Haynes 625 alloy, 50% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..