Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Tensile Strength, Yield | 120 MPa @Strain 0.200 %, Temperature 425 °C |
17400 psi @Strain 0.200 %, Temperature 797 °F |
Precipitation Hardened prior to test |
Special Metals INCOLOY® Alloy DS A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resista.. |
|||
Tensile Strength, Yield | 120 MPa @Temperature 300 °C |
17400 psi @Temperature 572 °F |
Annealed prior to test |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Tensile Strength, Yield | 120 MPa @Strain 0.200 %, Temperature 300 °C |
17400 psi @Strain 0.200 %, Temperature 572 °F |
Annealed prior to test |
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
Techmer ES Electrablend® PA6 GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA6.12 (Europe-Africa-Middle East) LNP THERMOCOMP* IF006 is a compound based on nylon 6/12 resin containing glass fibre |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Strength, Yield | 120 MPa @Thickness 3.17 mm |
17400 psi @Thickness 0.125 in |
ASTM D638 |
Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | GB/1040 |
Zhejiang Juner PA-A6-66H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide Applications: Cover of Mini MCBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram RamTough PZ307G6 Polycarbonate, 30% Glass Fiber, UV Stabilized 30% glass fiber reinforced polycarbonate, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Eurostar Staramide RF004XXC PA6, 20% Glass Fiber Filled, Injection Molded Staramide RF004XXC is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
E-Polymers TEKANATE™ G730FR , Flame Retardant, 30% Glass Fiber Reinforced Poly Carbonate 30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
Aclo Accutech Nylon 6 NY0730G20L Glass Reinforced |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Tensile Strength, Yield | 120 - 160 MPa | 17400 - 23200 psi | |
ArcelorMittal 06 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC06) and electroglavanized (DC06+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |
|||
Tensile Strength, Yield | >= 120 MPa | >= 17400 psi | Guaranteed Minimum L-T Direction; 0.2% Offset |
Aleris HOGAL 5558 Aluminum 5026-O/H111 HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |
|||
Tensile Strength, Yield | 120 - 180 MPa | 17400 - 26100 psi | |
ArcelorMittal 56+AS Aluminized steel Use: Extra-deep drawingInformation provided by ArcelorMittal |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
E-Polymers TEKAMID® TB120GM40 , 40% GF/MF Reinforced PA6, DAM 40% GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated. |