Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength, Yield | 119 MPa @Temperature 100 °C |
17300 psi @Temperature 212 °F |
ISO 527 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific) LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific) LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/M40 HS L BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackProc.. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/M40 IG BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedProcessing Method: In.. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific) LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL CN5258 PPE+PS (Asia Pacific) 40% filled FR high modulus PPE/PS blend |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK) TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels.. |
|||
Tensile Strength, Yield | 119 MPa @Temperature -40.0 °C |
17300 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8270 HS PA6 (Conditioned) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Tensile Strength, Yield | 119 MPa @Temperature -40.0 °C |
17300 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8270 HS PA6 (Conditioned) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | ASTM D638 |
Custom Resins Vexel™ 4200 RD PBT; 30% Glass Filler
(discontinued **) Property data for dry as molded samples.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 119 MPa | 17300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10 LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant. |