Polymer Property : Tensile Strength, Yield = 17250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 118.9 MPa
17250 psi
ASTM D638
Westlake Plastics Absylux® CN-F Acrylonitrile-Butadiene-Styrene (conductive)
Non-sloughing, carbon-fiber-filled material with high strength and stiffness; easily machined.Information provided by Westlake Plastics.