Tensile Strength, Yield 1.18 MPa
171 psi
ASTM D412
Microcell Composite Company CELLIFF® F7010 Polymer Foam
CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information pr..
Tensile Strength, Yield 1.18 - 35.0 MPa
171 - 5080 psi
Average value: 13.1 MPa Grade Count:65
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..