Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1160 - 1270 MPa | 169000 - 184000 psi | 3/4"x 0.030" Fiberglass Reinforced |
Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and.. |
|||
Tensile Strength, Yield | 1165 - 1172 MPa @Strain 0.200 % |
169000 - 170000 psi @Strain 0.200 % |
|
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.75 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Tensile Strength, Yield | 1165 MPa @Strain 0.200 % |
169000 psi @Strain 0.200 % |
|
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |