Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.15 MPa | 167 psi | ASTM D412 |
Polymax® Maxelast® P2620 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 1.15 MPa | 167 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-530 Dow-Corning Class VI Elastomer Information provided by Multibase |