Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 112 MPa | 16300 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/M55 L BK 15/40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight and Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat .. |
|||
Tensile Strength, Yield | 112 MPa | 16300 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF13 HS L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
Tensile Strength, Yield | 112 MPa | 16300 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF13 L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |