Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1110 MPa @Strain 0.200 % |
161000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 1110 MPa @Strain 0.200 % |
161000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |