Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON CP2100-KA02 PC+CF Description Injection Molding Grade, PC+CF, Electrostatic Dissipation, Low Surface ResistanceApplication: LCD Tray, HDD BracketCAS No. 103598-77-2 and 7440-44-0Information provided by LG Chemical |
|||
Tensile Strength, Yield | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
Tensile Strength, Yield | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical |
|||
Tensile Strength, Yield | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Greene Tweed Arlon® 1000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Tensile Strength, Yield | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Techmer ES HiFill® PA12 GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Techmer ES HiFill® PA12 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M36 HS BK 36% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 36% Filler by Weight and Mineral Filler, 36% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF10 TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(5%)Features: Lubricated, Good Wear Resistance, Low Fricti.. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Cheng Yu Plastic ML3425 PC, 25% Glass Fiber |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Cheng Yu Plastic NG1200S Nylon 66, 20% Glass Fiber Reinforced |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM D638 |
Cheng Yu Plastic FR200GV20 Flame Retardant Nylon 66, 20% Glass Fiber |
|||
Tensile Strength, Yield | 108 MPa | 15600 psi | ASTM 638 |
PlastxWorld CEVIAN® B2506 30% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |