Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1035 MPa | 150100 psi | 593°C Temper Temperature |
Latrobe Lescalloy® 4340 VAC-ARC ; 10.5" square High Strength Alloy Steel LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str.. |
|||
Tensile Strength, Yield | 1035 MPa @Strain 0.200 % |
150100 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Tensile Strength, Yield | 1035 MPa @Strain 0.200 % |
150100 psi @Strain 0.200 % |
|
ATI Allvac® 706 Nickel Superalloy, Heat Treatment: 954°C (1750°F) + Age Data provided by Allvac.Applications: Land based turbine wheels and spacers. Jet engine components. |
|||
Tensile Strength, Yield | >= 1035 MPa | >= 150100 psi | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H775 (H775) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Tensile Strength, Yield | >= 1035 MPa @Strain 0.200 % |
>= 150100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated plus Precipitation Heat Treated, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |