Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
NYCOA 2038 10% Glass Filled Nylon 6 10% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | |
Pacific Sintered Materials CU-143-W Copper Powdered Metal Applications: High electrical and thermal conductivity. Good for heat sinks and electrical components.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Polymer Resources TP-HG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy Polybutylene Terephthalate, 30% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | F5, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF20 IM2 BK 20% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF10 L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® PBT WM35 X Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Tensile Strength, Yield | 103 - 414 MPa | 15000 - 60000 psi | 0.2% offset |
Eagle Brass 735 Nickel Silver 18%, Annealed 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 103 - 172 MPa | 15000 - 25000 psi | |
Chicago Extruded Metals UNS C33500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in bars.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 103 - 172 MPa | 15000 - 25000 psi | |
Chicago Extruded Metals UNS C35000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 103 - 172 MPa | 15000 - 25000 psi | |
Chicago Extruded Metals UNS C35300 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Clariant Renol PA113G13 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Clariant Renol PA213G15 Nylon 6, 15% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 103 - 310 MPa | 15000 - 45000 psi | |
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-40FG-0684 40% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Asahi Kasei Thermofil N3-13FG-1626 13% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® MLS-20GF/000 Polysulfone Alloy - 20% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF5 HS 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, .. |
|||
Tensile Strength, Yield | 103 MPa | 15000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GFB20 20% Glass/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabiliz.. |