Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1030 - 1250 MPa | 149000 - 181000 psi | |
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 1030 - 1380 MPa | 149000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 1030 - 1280 MPa | 149000 - 186000 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Tensile Strength, Yield | 1030 MPa | 149000 psi | |
SSAB Tunnplat Domex® 034 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of .. |
|||
Tensile Strength, Yield | 1030 MPa | 149000 psi | |
SSAB Tunnplat Domex® 044 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | 1030 MPa | 149000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Tensile Strength, Yield | 1030 MPa | 149000 psi | Bar, Rod & Forgings |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |
|||
Tensile Strength, Yield | 1027 MPa | 149000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 1027 MPa | 149000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |