Tensile Strength, Yield 1025 MPa

@Strain 0.200 %
148700 psi

@Strain 0.200 %
Haynes 214® alloy, 20% cold reduction
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 1025 MPa

@Strain 0.200 %
148700 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 15% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..