Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.100 MPa
14.5 psi
JIS-K-6251(#2)/ASTM D-412
Fujipoly Industries Sarcon® GR-b Gap Filler Pad
Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
Tensile Strength, Yield 0.100 MPa
14.5 psi
JIS-K-6251(#2)/ASTM D-412
Fujipoly Industries Sarcon® GR-Hb Gap Filler Pad
Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
Tensile Strength, Yield >= 0.100 MPa
>= 14.5 psi
Unifrax CC-Max® 4 HP Substrate Support Mat
CC-Max 4 HP mat is produced when the proprietary fiber is converted into a flexible flet-like product. The material is thermally stable and engineered to maintain a controlled holding force on the ..
Tensile Strength, Yield >= 0.100 MPa
>= 14.5 psi
Unifrax IsoMat® AV/AVi Substrate Support Mat
Developed to meet the most stringent European regulatory requirements, IsoMat AV/Avi is engineered utilizing the unique Isofrax® 1260°C fibers - a revolutionary green fiber produced using patented..
Tensile Strength, Yield >= 0.100 MPa
>= 14.5 psi
Unifrax IsoMat® AV5 Substrate Support Mat
IsoMat AV5 is designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation.IsoMat AV5 offers superior performance at low tem..
Tensile Strength, Yield >= 0.100 MPa
>= 14.5 psi
Unifrax XPE® AV2/AV2i Substrate Support Mat
XPE®-AV2 is an advanced intumescent expanding mat designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation. When compa..
Tensile Strength, Yield >= 0.100 MPa
>= 14.5 psi
Unifrax XPE® MP Substrate Support Mat
XPE®-MP is a multipurpose, third-generation support mat system developed by Unifrax specifically for mechanical support and insulation of ceramic substrates used in diesel and gasoline emission con..
Tensile Strength, Yield >= 0.100 MPa
>= 14.5 psi
Unifrax XPE® NV Substrate Support Mat
XPE® intumescent mat products are designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation.Unifrax offers a variety of ..