Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.45 MPa | 1370 psi | ASTM D412 |
Polymax® Maxelast® C4760 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 9.45 MPa | 1370 psi | -10% change after 168 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N70N Nitrile Rubber Nitrile Butadiene Rubber (NBR) 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5595A Grade 70.Applications: Synthetic rubber resistant to petrole.. |
|||
Tensile Strength, Yield | 9.45 MPa @Strain 300 % |
1370 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3890E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |