Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 93.1 MPa | 13500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ MF 1200 A 40 HS Natural Polyamide 66 (Nylon 66) The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Tensile Strength, Yield | 93.2 MPa @Thickness 3.20 mm |
13500 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HTX1010F PEI (Asia Pacific) Higher impact, Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES Luriblend® TPX-PA6/6-01072 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific) LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA.. |
|||
Tensile Strength, Yield | 93.2 MPa | 13500 psi | ASTM D638 |
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF30 IM 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6 LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® PBT GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® PBT GF15 BK001 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: BlackTPCI# 6100111Information provided by TP Composit.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Tensile Strength, Yield | 93.2 MPa | 13500 psi | ASTM D638 |
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0687 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-20GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |