Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 86.0 MPa | 12500 psi | dry; ISO 527-1 |
Murtfeldt Murylon® 6 Cast Nylon 6 Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ASTM D638 |
NYCOA 512 PA 6 UL and NSF rated nucleated general purpose molding gradeInformation provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources NY66-EX1 High Viscosity Nylon 66 Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as .. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 80530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-033
(discontinued **) PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ISO value at 50 mm/min. |
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)
(discontinued **) Capron 5202 HS BK-102 is an unfilled, heat stabilized, pigmented black nylon 6,6, injection molding compound. It combines strength and stiffness as well as excellent chemical resistance. The additi.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ISO value at 50 mm/min. |
BASF Capron® 5202 HS Blend Nylon 66 (Dry)
(discontinued **) Capron 5202 HS Blend is a blended, unfilled, heat stabilized, nylon 6,6, injection molding compound. It is also available in natural and pigmented versions. It combines strength and stiffness as wel.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ISO value at 50 mm/min. |
BASF Capron® 8203C Nylon 6 (Dry)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D-638 |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF15 IM BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East) DATA ON BK1005 ONLY. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF5 L BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compos.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Techmer ES HiFill® PSU GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl PKN4717 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4717 is a PPO+PS concentrate for dilution with polystyrene resin for foam extrusion. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regu.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Europe-Africa-Middle East) NORYL PKN4752 is a translucent, high heat PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food cont.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10 LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | At 50 mm/min; ISO 527-2 |
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance.. |
|||
Tensile Strength, Yield | 86.2 MPa | 12500 psi | ASTM D638 |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ASTM D638 |
Entec Hypro™ PPC-GF40 Natural Impact Polypropylene, 40% Glass Reinforced Information provided by Entec |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 XEC1 POM Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe .. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | ISO value at 50 mm/min. |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | 50 mm/min |
Arkema Group Oroglas® V 044 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 044 is an extrusion grade offering good compromise between physical properties and thermal resistance.OROGLAS V 044 is recommended for extrusion of profiles, tubes and sheets.ISO data prov.. |
|||
Tensile Strength, Yield | 86.0 MPa | 12500 psi | 50 mm/min |
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion.. |