Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 850 - 1050 MPa | 123000 - 152000 psi | Swaged after Sintering |
MarkeTech 95-3-2 Tungsten Alloy, AMS-T-21014 Class 3 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 845 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
|
Haynes Multimet® alloy, 6.15 mm hot-rolled bar, 15% cold reduction Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Yield | 845 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
|
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 845 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
|
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 850 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals INCONEL® Alloy X-750 A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig.. |
|||
Tensile Strength, Yield | 850 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy 115 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It is similar to NIMONIC alloy 105 but has higher levels of aluminum and tit.. |
|||
Tensile Strength, Yield | >= 850 MPa | >= 123000 psi | After bake hardening |
SSAB Tunnplat Docol® 1000 DP High-strength Steel High-strength SteelCharacteristics: The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is.. |
|||
Tensile Strength, Yield | >= 850 MPa | >= 123000 psi | 80<x=100mm |
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength, Yield | 850 MPa | 123000 psi | 90º, RT, Dry; EN2561 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon Information provided by HexCel |
|||
Tensile Strength, Yield | 848 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
|
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 52% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Yield | 848 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Tensile Strength, Yield | 845 MPa | 123000 psi | Hardened 1800°F, Tempered 900°F |
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 850 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature after 10% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Tensile Strength, Yield | 845 MPa @Strain 0.200 % |
123000 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 482°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |