Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 8.34 MPa | >= 1210 psi | |
Kazanorgsintez 107-18 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Tensile Strength, Yield | >= 8.34 MPa | >= 1210 psi | |
Kazanorgsintez 107-19 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Tensile Strength, Yield | >= 8.34 MPa | >= 1210 psi | |
Kazanorgsintez 107-20 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Tensile Strength, Yield | >= 8.34 MPa | >= 1210 psi | |
Kazanorgsintez 107-22 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Tensile Strength, Yield | 8.34 MPa | 1210 psi | ASTM D412 |
Teknor Apex Flexalloy® 9800-60 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Tensile Strength, Yield | 8.34 MPa | 1210 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® X-590A-31 Thermoplastic Polyurethane Type: Estane® X-590A-31 is a Shore 91A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizo.. |
|||
Tensile Strength, Yield | 8.34 MPa | 1210 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® CR180A Thermoplastic Polyurethane Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Yield | 8.34 MPa | 1210 psi | 100%; ASTM D412 |
Teknor Apex APEX® 2580-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength, Yield | 8.34 - 20.7 MPa | 1210 - 3000 psi | Average value: 12.3 MPa Grade Count:53 |
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an.. |