Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Polymax® Maxelast® P3653T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | >= 8.27 MPa | >= 1200 psi | ASTM D638 |
S&E Specialty Polymers GTPO8290-GT7 PVC Application: 80°C, Low Smoke, Zero Halogen, Flame Retardant Polyethylene Compound for extrusion applications. Specifically designed to withstand severe UV exposure while maintaining very good .. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Polymax® Maxelast® C4880 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 20 in/min, injection molded, type 1 specimen; ASTM D638 |
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin
(discontinued **) Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 500 mm/min; ASTM D638 |
Eastman D4056-P Polyethylene
(discontinued **) Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no lon.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | |
Kraton® D1102 + LDPE blend (20/80) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7455 ER TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Tensile strength decreases by 25% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 9275 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex APEX® 3201-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex APEX® 3210-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex APEX® 3301-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3302-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | 100%; ASTM D412 |
Teknor Apex MF 165 D NT Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2840M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2850E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | >= 8.27 MPa | >= 1200 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7157 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex TEKBOND® MP 1728 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex TEKBOND® MP 1728 UVF Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tensile Strength, Yield | 8.30 MPa @Strain 100 % |
1200 psi @Strain 100 % |
ASTM D638 |
Toyobo E3090A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information .. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.27 MPa @Temperature 166 °C |
1200 psi @Temperature 330 °F |
Flatwise Tensile; Control; Thermal Cycling |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Softflex® SF 5560 Overmold for Nylon Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | |
Dow AFFINITY™ SM 1350 Polyolefin Plastomer AFFINITY® SM 1350 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in durable injection molded housewares and compression molded closure liners or gaskets. It exhibit.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | Molded property |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | ASTM D-638 |
Axiall 8542 Moldings & Extrusions Flexible PVC General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 8.30 - 21.0 MPa | 1200 - 3050 psi | Average value: 11.5 MPa Grade Count:59 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Yield | 8.27 MPa | 1200 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 38-074 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:Hot Runner MoldingFDA (Food Contact)Teething ring & pacifierMulti-PurposeMarket:Consumer GoodsProcessing Method:I.. |