Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 780 MPa @Strain 0.200 % |
113000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy 80A A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a.. |
|||
Tensile Strength, Yield | 780 MPa | 113000 psi | |
SSAB Tunnplat Domex® Wear Steel Sheet Domex® Wear is a new grade of steel sheet in the Domex® range, and its main distinguishing features are good wear resistance, high strength, good bendability, high toughness and good weldabili.. |
|||
Tensile Strength, Yield | 780 MPa @Strain 0.200 % |
113000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Tensile Strength, Yield | 779 MPa @Strain 0.200 % |
113000 psi @Strain 0.200 % |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Tensile Strength, Yield | 780 MPa @Strain 0.200 % |
113000 psi @Strain 0.200 % |
|
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |
|||
Tensile Strength, Yield | 780 MPa @Strain 0.200 % |
113000 psi @Strain 0.200 % |
|
Haynes 556® alloy, 20% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 780 MPa @Strain 0.200 % |
113000 psi @Strain 0.200 % |
|
Haynes 625 alloy, 10% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |