Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 75.8 MPa | 11000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 1280 A HS Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
Nylene® Norpex® AX300 PPE (Polyphenylene Ether); Premium Performance High Heat Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 LNP* COLORCOMP* PX99848 is an unfilled Nylon 6 resin. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 (Asia Pacific) LNP* Colorcomp* PX99848 is a compound based on Nylon 6 resin containing Unfilled Custom Color. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR QD 818.Y001 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 75.8 - 127 MPa | 11000 - 18400 psi | Average value: 107 MPa Grade Count:11 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP G1000 PSU (Europe-Africa-Middle East) LNP* COLORCOMP* G1000-GY4A805-0 is a compound based on Polysulfone resin. Added features include: Custom Color Grey. |
|||
Tensile Strength, Yield | 76.0 MPa @Temperature 22.0 °C |
11000 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Tensile Strength, Yield | 75.86 MPa | 11000 psi | ASTM D638 |
Lucent Polymers GPP-130 Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/M25 HS L BK 25% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF6 UG BK MB 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Low Viscosity and LubricatedProcessing Method: Injection MoldingInformation provided by TP .. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Plastiblend® TPX-HTN-000CA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES Luriblend® POM CO CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated and CopolymerUL File: E157318Information provided b.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO 527-1/-2 |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | |
Covestro Makroblend® UT-620 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Ensinger Tecamid® MDS® Molybdenum Disulfide Filled Nylon (PA) Tecamid MDS® has enhanced surface lubricity and wear resistance over unfilled nylon. It is an ideal material to replace metals in machinery. Low surface friction Increased surface hardness Incre.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6) VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety .. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Clariant Renol 612G10-L Nylon 612, 10% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 75.8 - 427 MPa | 11000 - 62000 psi | |
Chicago Extruded Metals BioBrass® UNS C22600 Copper-Zinc Alloy Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Clariant Renol 66B40 Nylon 66, 40% Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0709 30% Fiber Glass Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Asahi Kasei Thermylene® P7-20FG-0610 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 76.0 MPa | 11000 psi | ISO value at 50 mm/min. |
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur.. |
|||
Tensile Strength, Yield | 75.8 MPa | 11000 psi | ASTM D638 |
Techmer ES HiFill FR® PPO/HIPS MM20 FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by Weight Features: Flame RetardantInformation provided by TP Composites, Inc. |