Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.700 MPa | 102 psi | ISO 37* |
Premix Thermoplastics PRESEAL® TPE 6071 PRESEAL TPE 6071 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp.. |
|||
Tensile Strength, Yield | 0.700 MPa | 102 psi | JIS-K-6251(#2)/ASTM D-412 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Tensile Strength, Yield | 0.700 MPa | 102 psi | 150°C for 1,000 hrs; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Tensile Strength, Yield | 0.703 MPa | 102 psi | As manufactured |
Unifrax Fiberfrax® 550 Ceramic Fiber Paper 550 paper is made from unwashed high-purity ceramic fiber. Its higher density and binders give performance properties ideal for most refractory applications.Information Provided by Unifrax I LLC |