Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 69.0 MPa | 10000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® INP563 ABS SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t.. |
|||
Tensile Strength, Yield | >= 68.9 MPa | >= 10000 psi | Clear Casting |
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding
(discontinued **) TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | ASTM Data |
Dow Isoplast® 202 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 202 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | ISO value at 50 mm/min. |
BASF Capron® 1943 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 1943 is a type 6 nylon graft copolymer developed for injection molding applications requiring improved dry as molded toughness, and increased flexibility. It has an excellent thermal and che.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF5 HS BK002 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided b.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES HiFill® PEEK HF Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, .. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant Features: Lubricated, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Westlake Plastics Ardel® Polyarylate Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Yield | 69.0 MPa @Temperature 23.0 °C |
10000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Clariant PCSP0014 GREY Polycarbonate, Stainless Steel Fiber, EMI Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-2153 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Asahi Kasei Thermylene® P1-20FG-2703 20% Glass Fiber Reinforced, Impact Modified Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® 540Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 69.0 MPa | 10000 psi | ASTM D638 |
Ashley Polymers Ashlene® 747 Nylon 6/66 A medium viscosity copolymer. Excellent flexibility and elongation suitable for film and monofilament applications.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 68.97 MPa | 10000 psi | ASTM D638 |
Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |