Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 45.0 - 65.0 MPa | 6530 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Tensile Strength, Yield | 40.0 - 65.0 MPa | 5800 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Tensile Strength, Yield | 45.0 - 65.0 MPa | 6530 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Tensile Strength, Yield | 45.0 - 65.0 MPa | 6530 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Tensile Strength, Yield | 40.0 - 65.0 MPa | 5800 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Tensile Strength, Yield | 45.0 - 65.0 MPa | 6530 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Tensile Strength, Yield | 13.0 - 65.0 MPa | 1890 - 9430 psi | Average value: 41.4 MPa Grade Count:92 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Tensile Strength, Yield | 60.0 - 65.0 MPa | 8700 - 9430 psi | Average value: 63.1 MPa Grade Count:17 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Yield | 64.0 - 65.0 MPa | 9280 - 9430 psi | ASTM D638 |
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 250 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 250 system.Typical ApplicationsMulti-purpose modelsRTV mold patternsForm/Fit/.. |
|||
Tensile Strength, Yield | 35.0 - 65.0 MPa | 5080 - 9430 psi | Average value: 50.0 MPa Grade Count:13 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |