Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 450 - 620 MPa | 65300 - 89900 psi | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Tensile Strength, Yield | 500 - 620 MPa @Strain 0.200 % |
72500 - 89900 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 500YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Tensile Strength, Yield | 551 - 620 MPa @Strain 0.200 % |
79900 - 89900 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TD04 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 482 - 620 MPa @Strain 0.200 % |
69900 - 89900 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TM00 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |