Mechanical Properties Metric English Comments
Tensile Strength, Yield 540 - 610 MPa

@Strain 0.200 %
78300 - 88500 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..