Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 483 - 552 MPa @Strain 0.200 % |
70000 - 80000 psi @Strain 0.200 % |
|
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 441 - 552 MPa | 64000 - 80000 psi | 0.2% offset |
Eagle Brass 18665 MSP1, Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Yield | 503 - 552 MPa | 73000 - 80000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, Extra Spring CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 462 - 552 MPa | 67000 - 80000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 441 - 552 MPa | 64000 - 80000 psi | 0.2% offset |
Eagle Brass 511 Phosphor Bronzes 4%, 3/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |