Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 407 - 462 MPa | 59000 - 67000 psi | 0.2% offset |
Eagle Brass 210 Gilding Metal, Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Yield | 414 - 462 MPa | 60000 - 67000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, Extra Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |