Tensile Strength, Yield 352 - 407 MPa
51000 - 59000 psi
0.2% offset
Eagle Brass 151 ZHC® COPPER, Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Tensile Strength, Yield 296 - 407 MPa
43000 - 59000 psi
0.2% offset
Eagle Brass 18665 MSP1, 1/4 Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Tensile Strength, Yield 303 - 407 MPa
44000 - 59000 psi
0.2% offset
Eagle Brass 19210 XP-10 Copper Iron, 1/2 Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Tensile Strength, Yield 110 - 407 MPa
16000 - 59000 psi
0.2% offset
Eagle Brass 194 HSM® Copper, Annealed
High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl..
Tensile Strength, Yield 338 - 407 MPa
49000 - 59000 psi
0.2% offset
Eagle Brass 220 Commercial Bronze, 3/4 Hard
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..