Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 300 - 360 MPa @Strain 0.200 % |
43500 - 52200 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 300 RP High-strength Steel High-strength SteelComments: Docol RP - Cold Rolled Steel - rephosphorized steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.0 mm. Iron content is approximate - exact compositi.. |
|||
Tensile Strength, Yield | 170 - 360 MPa | 24700 - 52200 psi | |
ArcelorMittal 11 High formability steel for drawing, Hot rolled Available in the following: uncoated (DD11) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au.. |
|||
Tensile Strength, Yield | 300 - 360 MPa | 43500 - 52200 psi | |
ArcelorMittal 300 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC300B), electroglavanized (HC300B+ZE) and Extragal®/Galvannealed (HC300BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Yield | 300 - 360 MPa | 43500 - 52200 psi | |
ArcelorMittal H 360 Solid solution steel, Cold rolled Available in the following: uncoated (HC300P) and electrogalvanized (HC300P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |
|||
Tensile Strength, Yield | 300 - 360 MPa | 43500 - 52200 psi | |
ArcelorMittal HSLA 300 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC300LA), electroglavanized (HC300LA +ZE) and Extragal®/galfan/Galvannealed (HC300LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |