Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.0 - 35.0 MPa | 2030 - 5080 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Tensile Strength, Yield | 14.0 - 35.0 MPa | 2030 - 5080 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Tensile Strength, Yield | 8.80 - 35.0 MPa | 1280 - 5080 psi | Average value: 19.4 MPa Grade Count:34 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Yield | 20.0 - 35.0 MPa @Thickness 2.00 mm |
2900 - 5080 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Tensile Strength, Yield | 14.0 - 35.0 MPa @Thickness 2.00 mm |
2030 - 5080 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Tensile Strength, Yield | 14.0 - 35.0 MPa @Thickness 2.00 mm |
2030 - 5080 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Tensile Strength, Yield | 22.0 - 35.0 MPa | 3190 - 5080 psi | Spec; ISO 527-1/2 |
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co.. |
|||
Tensile Strength, Yield | 20.0 - 35.0 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
2900 - 5080 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Tensile Strength, Yield | 14.0 - 35.0 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
2030 - 5080 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Tensile Strength, Yield | 30.0 - 35.0 MPa | 4350 - 5080 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Tensile Strength, Yield | 1.18 - 35.0 MPa | 171 - 5080 psi | Average value: 13.1 MPa Grade Count:65 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |