Mechanical Properties Metric English Comments
Tensile Strength, Yield 170 - 320 MPa
24700 - 46400 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 170 - 320 MPa
24700 - 46400 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 260 - 320 MPa

@Strain 0.200 %
37700 - 46400 psi

@Strain 0.200 %
SSAB Tunnplat Aluzink 260A RP-X High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink RP - rephosphorized steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.5 - 1.5 mm. Iron content is approximate - exact compo..
Tensile Strength, Yield 260 - 320 MPa

@Strain 0.200 %
37700 - 46400 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 260 RP High-strength Steel
High-strength SteelComments: Docol RP - Cold Rolled Steel - rephosphorized steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.0 mm. Iron content is approximate - exact compositi..
Tensile Strength, Yield 250 - 320 MPa

@Strain 0.200 %
36300 - 46400 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 400DP High-strength Steel
High-strength SteelComments: Docol DP - Cold Rolled Steel - dual-phase steel. Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact composition is..
Tensile Strength, Yield 260 - 320 MPa

@Strain 0.200 %
37700 - 46400 psi

@Strain 0.200 %
SSAB Tunnplat Dogal 260 RP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat.
Tensile Strength, Yield 260 - 320 MPa

@Strain 0.200 %
37700 - 46400 psi

@Strain 0.200 %
SSAB Tunnplat Dogal 260 RP-X High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat.
Tensile Strength, Yield 260 - 320 MPa
37700 - 46400 psi
ArcelorMittal H 260 Solid solution steel, Cold rolled
Available in the following: uncoated (HC260P) and electrogalvanized (HC260P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste..
Tensile Strength, Yield 260 - 320 MPa
37700 - 46400 psi
ArcelorMittal HSLA 260 High strength low alloy steel for cold forming, Cold Rolled