Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.5 - 29.4 MPa | 3560 - 4270 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Tensile Strength, Yield | 24.5 - 29.4 MPa | 3560 - 4270 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |