Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 276 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 241 - 276 MPa

@Strain 0.200 %
35000 - 40000 psi

@Strain 0.200 %
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 241 - 276 MPa

@Strain 0.200 %
35000 - 40000 psi

@Strain 0.200 %
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 138 - 276 MPa

@Strain 0.200 %
20000 - 40000 psi

@Strain 0.200 %
Materion ToughMet® T3 CA
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Tensile Strength, Yield 124 - 276 MPa
18000 - 40000 psi
0.2% offset
Eagle Brass 240 Low Brass, 1/4 Hard
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..
Tensile Strength, Yield 193 - 276 MPa
28000 - 40000 psi
0.2% offset
Eagle Brass 519 Phosphor Bronzes 6%, Annealed
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Yield 110 - 276 MPa
16000 - 40000 psi
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy
Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extrude..
Tensile Strength, Yield 207 - 276 MPa
30000 - 40000 psi
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 303, Annealed (UNS S30300)
Allegheny Ludlum's 303 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..