Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 133 - 230 MPa | 19300 - 33400 psi | Average value: 173 MPa Grade Count:8 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Yield | 15.0 - 230 MPa | 2180 - 33300 psi | Average value: 114 MPa Grade Count:48 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Tensile Strength, Yield | 55.0 - 230 MPa | 7980 - 33400 psi | Average value: 184 MPa Grade Count:94 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Tensile Strength, Yield | 152 - 230 MPa | 22000 - 33400 psi | Average value: 183 MPa Grade Count:6 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Tensile Strength, Yield | 140 - 230 MPa | 20300 - 33400 psi | Average value: 170 MPa Grade Count:10 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Yield | 180 - 230 MPa | 26100 - 33400 psi | |
ArcelorMittal 03 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC01) and electroglavanized (DC01+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |
|||
Tensile Strength, Yield | 180 - 230 MPa | 26100 - 33400 psi | |
ArcelorMittal 180 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC180B), electroglavanized (HC180B+ZE) and Extragal®/Galvannealed (HC180BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Yield | 180 - 230 MPa | 26100 - 33400 psi | |
ArcelorMittal IF 180 High strength IF steel, Cold rolled Available in the following: uncoated (HC180Y), electroglavanized (HC180Y+ZE) and Extragal®/Galvannealed (HX180YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Tensile Strength, Yield | 180 - 230 MPa | 26100 - 33400 psi | |
ArcelorMittal 53 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX53D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |