Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.827 - 23.4 MPa | 120 - 3400 psi | Average value: 11.1 MPa Grade Count:379 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Tensile Strength, Yield | 17.5 - 23.4 MPa | 2540 - 3390 psi | Average value: 21.2 MPa Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |