Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.965 - 2137 MPa

@Temperature -59.0 - 177 °C
430.0 - 309900 psi

@Temperature -74.2 - 351 °F
Average value: 945 MPa Grade Count:19
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..