Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1517 - 1689 MPa | 220000 - 245000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | 1655 - 1689 MPa @Strain 0.200 % |
240000 - 245000 psi @Strain 0.200 % |
302°C Temper Temperature |
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel LESCALLOY 300M VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and tou.. |